1. First remove the sludge from the surface of the broken weld screw head barrage will be the center of the Section barrage dead and then with an electric drill on the diameter of 6-8 mm drill bit in the center of the Section barrage hole drilling, pay attention to the hole must be drilled through. After drilling through the hole, remove the small drill bit, replace the drill bit with a diameter of 16 mm, continue to expand the hole of the broken bolt and drill through.
2. Take the electrode with a diameter of less than 3.2 mm using the small and medium current in the hole of the broken bolt from the inside to the outside of the surfacing surfacing to remove the entire length of the bolt half can be. When starting surfacing, the arc should not be too long to avoid burning the outer wall of the broken bolt. After surfacing to the upper surface of the broken bolt, the surfacing of 1 cylinders with a diameter of 14-16 mm and 8-10 mm is continued to be welded.
3. After the surfacing is welded, hammer the end surface with hammer to cause the broken head bolt to vibrate along its axis. Since the heat generated by the previous arc and subsequent cooling, coupled with the vibration at this time, can cause loosening between the break bolt and the thread of the body.
4. Carefully observe the M18 nut sleeve on the surfacing stigma and weld the two when a trace amount of rust is found leaking from the fracture.
5. After welding slightly cool and hot with plum wrench sleeve on the nut left and right twist can also be twisting back and forth with a small hammer knock nut end so that the broken bolt can be removed. 6. After removing the broken bolt, use the appropriate taps to process the wire buckle inside the rack to remove rust and other debris from the hole.